This product is an aluminum-copper master alloy containing 48.0-52.0% copper, which is used for adding copper elements in aluminum alloy smelting. The addition temperature is low and the composition control is accurate.
How to use:
1. Bake and dry before use.
2. Adding temperature: above 680°C.
3. The dosage of this product is determined by calculation and experiment according to the actual situation.
4. Adding method: remove the scum, lightly pour this product into molten aluminum, stir evenly after melting, sample and analyze, and pour after the composition is qualified.
Packaging and storage:
This product is in block or waffle shape with metallic luster, see the table below for specific specifications:
Shape |
Specification |
Packing |
Measurement |
block |
400g/piece |
Cardboard box |
25±0.25kg/piece |
Waffle shape |
7.5~9kg/piece |
pallet |
tons |
Store in a ventilated and dry place, away from moisture.